boat bottom paint blisters
Once it is completely cured, wash the repaired area with soap and water. the repair is now ready to be sanded and painted with sea hawk bottom paint. if redoing the hull apply tuff stuff primer, followed by bottom paint. if the blister has damaged the fiberglass, that will need to be repaired with fiberglass cloth cut to match damaged area.. Stage 3 – blister formation. the effect of more water continuously being pulled into the cell is a rise in pressure leading to swelling and blistering as is most often seen on affected hulls. stage 4 – laminate failure. eventually some of the blisters will rupture leading to liquid seeping out of them.. Zyrex original bottom boat paint formula – since 1988 for cooler waters rubberized co-polymer epoxy environmentally friendly – legal world wide water proof – blister prevention 5-10 years between applications – to refresh growth prevention additive includes primer & bearer coat same weight as water.
boat bottom paint blisters